Ah, I've never used sulfuric at a concentration that high before. It's rather hard to get in NJ. The purest I can get is from Rooto, and that has the organic inhibitors in it, so you have to add a little water and heat to make it do much of anything to metal.

I will finally be able to get a gallon of concentrated, so it's good to know this additional detail. So I could use a steel mesh strainer to separate the base metal bits from the gold particles. Hmmm, how does one go about separating the larger pieces of gold foil with this method?
Mild Steel is Ok, I do not know how well alloyed Steel hold up.
The Gold particles will be under the Copper mesh, so why do you want to use a strainer?
 