hi guys,
so im trying to get the perfect shiny gold ingots every single time. and currently we only get it sometimes
ive optimized by procedure using the tips seen around the forum such as double AR and washing with HCL and/or Nitric. I chose nitric because HCL just doesnt work for me.
im only interested in the ever lasting gold shine that people care about thats whats important.
so ive almost perfected the procedure currently i do the following
Double Refining with AR and SMB to percipitate then;
1.Wash with ammonia (15mins)
2. Wash with Nitric 35% (15mins)
3.Wash With Ammonia (15Mins)
4. Wash With Nitric 35% (15mins)
5. Wash with Ammonia (15mins)
6. Wash With Nitric (10mins)
7. Distilled Hot Water x 3 Washes
i mean even after all this its still a hit and miss 50/50 could anyone suggest something to get that superb glow all around the ingot not just in certain places. what provides the glow? cause ive even seen 99.5% gold bars that are shiny so what could it be?
any suggestions guys
so im trying to get the perfect shiny gold ingots every single time. and currently we only get it sometimes
ive optimized by procedure using the tips seen around the forum such as double AR and washing with HCL and/or Nitric. I chose nitric because HCL just doesnt work for me.
im only interested in the ever lasting gold shine that people care about thats whats important.
so ive almost perfected the procedure currently i do the following
Double Refining with AR and SMB to percipitate then;
1.Wash with ammonia (15mins)
2. Wash with Nitric 35% (15mins)
3.Wash With Ammonia (15Mins)
4. Wash With Nitric 35% (15mins)
5. Wash with Ammonia (15mins)
6. Wash With Nitric (10mins)
7. Distilled Hot Water x 3 Washes
i mean even after all this its still a hit and miss 50/50 could anyone suggest something to get that superb glow all around the ingot not just in certain places. what provides the glow? cause ive even seen 99.5% gold bars that are shiny so what could it be?
any suggestions guys