A Anonymous Guest Feb 6, 2008 #1 Will the gold cell work for silver plate? I would biuld one but if it does not for for silver plate I really could not use it. thanks Jim
Will the gold cell work for silver plate? I would biuld one but if it does not for for silver plate I really could not use it. thanks Jim
draftinu Well-known member Joined Dec 10, 2007 Messages 85 Location kenosha Feb 6, 2008 #2 I am interested also.
Harold_V Well-known member Moderator Emeritus Joined Feb 25, 2007 Messages 8,360 Feb 7, 2008 #3 Sulfuric cells will strip silver. Do a search on this forum, or check the posts by gold silver pro-----one of them will include the patent number, which will allow you to read about the basic operation and capability of these cells. Harold