lazersteve
Well-known member
All,
I decided to start a new series of posts detailing the yields of harvesting various scrap items.
The first installment in this series will be the yield data on network cards like this one:
I determined this information based upon two hundred and fourteen 3Com 3c509TP Etherlink III ISA ethernet network cards with RJ45 and AUI connectors.
Here's the box of the 214 cards after the fingers and AUI pins were removed:
Here's an overview of the before and after shots:
Now for the yield information:
The 214 cards yielded 600 grams of fingers and 125 grams of gold plated pin tips from the 16 pin AUI connectors. The fingers are in the large bag in the photo above and the AUI gold tips are in the quart sized bag. The small bag contains the unplated portions of the AUI pins and weighs 64 grams.
Every 5 cards weighed 15.8 ounces (~1 LB) and yielded 14 grams of clean cut fingers.
28 grams (1 ounce) of fingers (10 cards worth) produced the foils seen in the jar in the upper right corner of the photo above. Here's a closeup of the foils:
I haven't melted and weighed the foils yet, but I will update this post with a photo of the gold BB they form and a weight for the BB.
Additionally, I'll be filming portions of the processing of the fingers pictured here to demonstrate the process in detail for everyone.
My next installment will show yield data for slotted processors.
Steve
I decided to start a new series of posts detailing the yields of harvesting various scrap items.
The first installment in this series will be the yield data on network cards like this one:
I determined this information based upon two hundred and fourteen 3Com 3c509TP Etherlink III ISA ethernet network cards with RJ45 and AUI connectors.
Here's the box of the 214 cards after the fingers and AUI pins were removed:
Here's an overview of the before and after shots:
Now for the yield information:
The 214 cards yielded 600 grams of fingers and 125 grams of gold plated pin tips from the 16 pin AUI connectors. The fingers are in the large bag in the photo above and the AUI gold tips are in the quart sized bag. The small bag contains the unplated portions of the AUI pins and weighs 64 grams.
Every 5 cards weighed 15.8 ounces (~1 LB) and yielded 14 grams of clean cut fingers.
28 grams (1 ounce) of fingers (10 cards worth) produced the foils seen in the jar in the upper right corner of the photo above. Here's a closeup of the foils:
I haven't melted and weighed the foils yet, but I will update this post with a photo of the gold BB they form and a weight for the BB.
Additionally, I'll be filming portions of the processing of the fingers pictured here to demonstrate the process in detail for everyone.
My next installment will show yield data for slotted processors.
Steve