Harold, and others that have grown silver crystal, is there a electro process that will grow gold crystals from a solution? Just saw one that God made and wondered if we could do something 10% that good would be awesome. :lol:
Wyndham
 
Wyndham said:
is there a electro process that will grow gold crystals from a solution?
I am not aware of a process that yields crystals. Everything I've read regards a gold cell indicates gold plates out in nodules.

While I had built a small gold cell, capacity of approximately 20 troy ounces, I never put it in service, so I have no experience with parting gold electrolytically.

Interesting question! :wink:

Harold
 
Try electroforming. It is made
with cyanide solution. Theoretically
you need to work without brighterners
which introduce embrittlement. Best
use proprietary formulation
 
I was doing some experiments in crystallization once and decided to try it on a gold chloride solution. I added salt (sodium chloride) and cooked the solution down. As the solution reached saturation crystals began to form out of the solution and I had no problem filtering. Just a thought.

Randy in Gunnison
 
Randy, were these solid gold and was this a pinch of salt or about how much. Thats for the idea it might also work with a current like the silver does.
Wyndham
 
I was working from a gold chloride solution and I just threw in a handful of coarse rock salt, dissolve it, and started boiling the solution to saturation. No electrolysis was involved. This is what I do to make a deep reddish brown RhCl(2) and sometimes the rhodium comes out blood red.