So I had some gold foils. I added HCl to the foils until it covered the top of he foils. Then added bleach in small increments until the foils dissolved...all merry and good.
Then I added SMB to the solution to drop the gold. Nothing happening. I kept adding more and more SMB and I'm pretty sure I've added way to much. But when I test the solution with stannous chloride, the solution still turns a very dark brown ( almost black). But there is still no gold dropping. Not sure what's going on. Could someone help me?
So I had some gold foils. I added HCl to the foils until it covered the top of he foils. Then added bleach in small increments until the foils dissolved...all merry and good.
Then I added SMB to the solution to drop the gold. Nothing happening. I kept adding more and more SMB and I'm pretty sure I've added way to much. But when I test the solution with stannous chloride, the solution still turns a very dark brown ( almost black). But there is still no gold dropping. Not sure what's going on. Could someone help me?