All,
I processed 160g of gold fingers removed from misc telecomm boards, using cyanide leaching and recovered 0.4g of purfied gold powder. Here are some photos,
Starting materials,
Materials after leaching completed within few seconds,
Here is the gold powder precipitated from cyanide leaching, gold recovered from fingers usually very fine form,
Refine gold powder,
Once again I would like to thank the forum members specially GoldSilverPro and Jaun whose their posts have been helping me learn about cyanide leach.
Regards
Kj
I processed 160g of gold fingers removed from misc telecomm boards, using cyanide leaching and recovered 0.4g of purfied gold powder. Here are some photos,
Starting materials,
Materials after leaching completed within few seconds,
Here is the gold powder precipitated from cyanide leaching, gold recovered from fingers usually very fine form,
Refine gold powder,
Once again I would like to thank the forum members specially GoldSilverPro and Jaun whose their posts have been helping me learn about cyanide leach.
Regards
Kj