Anodizing is usually done with some chemical, one such is iodine which imparts a golden color while reducing wear by increasing oxide layer. "The most common anodizing processes on aluminium use chromic acid, sulfuric acid or oxalic acid (Wernick et al., 1987). Other acids, such as phosphoric acid and boric sulfuric acid mix, are now used in the market for anodizing in the aerospace industry." The most common anodizing processes on aluminium use chromic acid, sulfuric acid or oxalic acid (Wernick et al., 1987). Other acids, such as phosphoric acid and boric sulfuric acid mix, are now used in the market for anodizing in the aerospace industry.