Hello!
What are your experiences with gold plated flatware? How much gold is on spoons and forks?
Modern gold plated flatware is made of steel. That makes it very easy to recover the gold - simply put it in the furnace and heat to 1200°C.
regards
What are your experiences with gold plated flatware? How much gold is on spoons and forks?
Modern gold plated flatware is made of steel. That makes it very easy to recover the gold - simply put it in the furnace and heat to 1200°C.