copperkid_18 Well-known member Joined Feb 25, 2010 Messages 193 Location Ellis, Kansas Jan 5, 2011 #1 I was wondering what the best way ( easiest for me) to process gp'd steel scrap. Hot HCL? AP? Thanks, Kobe Attachments IMG_2752.JPG 1.5 MB
I was wondering what the best way ( easiest for me) to process gp'd steel scrap. Hot HCL? AP? Thanks, Kobe
lazersteve Well-known member Moderator Emeritus Joined Feb 27, 2007 Messages 7,334 Location Florida Jan 5, 2011 #2 Looks like very lightly plated stuff, the cell will strip them down in a heartbeat. You won't get enough gold to process so I would save them up until you have a pound or more of similar scrap. Steve
Looks like very lightly plated stuff, the cell will strip them down in a heartbeat. You won't get enough gold to process so I would save them up until you have a pound or more of similar scrap. Steve