Dissolve processor in AR .processor is consist of steel leg plated with gold iron in processor it means hard to recover gold from processor when processor dissolve in AR then evaporate all AR convert into dry encrust then add HCL for convert nitrite into chloride evaporate whole HCL to dry encrust then add HCL to dissolve base metals
With iron . filter this HCL which is base metal chlorides remains powder which is consist of gold then make AR dissolve this powder neutralized and precipitate with SMB and you get pure gold.... WHAT YOU THINK ABOUT MY IDEA…… :idea:
 
Your process looks good,but if you are processing a gold plated steel leg,then you should consider using the electrolytic cell instead.More efficient,faster and cheaper for what you are processing.