I have gray powder after I did my first recovery mixed with the gold flakes. How do I get rid of it. I used the vinegar salt peroxide method to recover the foils.
 
You need to give us more information such as what you were processing .
As a side question why did you use vinegar and salt instead of HCl ?
 
You need to give us more information such as what you were processing .
As a side question why did you use vinegar and salt instead of HCl ?
I didn’t have any HCL and was trying to do it it a little more disposal friendly. I was recovering from ram sticks and other cell phone parts.
 
I didn’t have any HCL and was trying to do it it a little more disposal friendly. I was recovering from ram sticks and other cell phone parts.
The moment it has dissolved metals it is no longer disposable friendly.
Actually salts from Vinegar may pose greater danger as Acetic acid is an organic acid.
 
I have gray powder after I did my first recovery mixed with the gold flakes. How do I get rid of it. I used the vinegar salt peroxide method to recover the foils.
This still makes a weak and often dirty hydrochloric acid. And is still not any easier to make "disposal safe".

Yggdrasil beat me to it, but...
 
I have gray powder after I did my first recovery mixed with the gold flakes. How do I get rid of it. I used the vinegar salt peroxide method to recover the foils.
Welcome to us bye the way.

Here are some links we recommend to study:

We ask our new members to do 3 things.
1. Read C.M. Hokes book on refining jewelers scrap, it gives an easy introduction to the most important chemistry regarding refining.
It is free here on the forum: https://goldrefiningforum.com/phpBB3/viewtopic.php?f=54&t=19798
2. Then read the safety section of the forum: https://goldrefiningforum.com/forums/safety.47/
3. And then read about "Dealing with waste" in the forum: https://goldrefiningforum.com/threads/dealing-with-waste.10539/

Suggested reading:
https://goldrefiningforum.com/forums/the-library.101/
https://goldrefiningforum.com/threads/when-in-doubt-cement-it-out.30236/
https://goldrefiningforum.com/threa...le-read-this-before-you-post-about-ore.33333/


Forum rules is here.
https://goldrefiningforum.com/threads/gold-refining-forum-rules.31182/
 

Latest posts

Back
Top