Gold on PCBs is almost always plated onto a nickel layer over copper. So if you dissolve the copper using the acid peroxide (AP) method, there should always be nickel on the backside of the flakes. If the gold plating was relatively thin (good ones are 8 µm to 16 µm), you'll get proportionally more nickel compared to thicker gold-plated traces.