TheArchitect
Member
After i filter and dry the solids from the Sulfuric Cell...can the dry Au powder be disolved in HCl-CL and then filtered again... in the same manner of treating the gold foils from stripped fingers?
Thanks.
Thanks.
Rag and Bone said:Could it be cleaned before dissolving? Clean gold dissolves and drops soooo nicely.