All,
Tonight the hammer mill prototype completed, tested and results were satisfactory. Motor is 3-phase, 380V, 3000rpm, and it has 3hp. There are 3 blades, made from car suspension, 2 of them crossed shape while the 3rd one sits on the others, is U shaped to help with better milling.
This is what the inside looks like,
This is an overall shot of the hammer mill,
This is the result from milling the pyrolyzed ICs.
Best regards,
Kj