y
If there's gold in there it can't escape :)
If it's colloidal, maybe time passing will have allowed it to flocculate. You could try to filter it again to see what you get.
But to be realistic, if you didn't crush your material at the start, the gold is still hidden inside the chips. I would look into that first. Do you still have the material you processed?
es i still have the material i processed im going to shred some of it and jaw crush some of it to see what has the best returns as i know there is some gold still inside of the items
 