(Help!!!) (Platinum?) (Palladium)? (Copper?) (Rodium?) Stanous Chloride Test? Catalytic converter chlorine leach solution?

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

chris1977impala1

New member
Joined
Sep 29, 2024
Messages
1
Location
Junction City Oregon
1000000918.jpg can somebody please tell me what I have in solution? This is a status chloride test That I used on a catalytic converter. Substrate chlorine leach solution!
 

Attachments

  • PXL_20241008_012905323.jpg
    PXL_20241008_012905323.jpg
    1.6 MB
  • PXL_20241008_012759888.jpg
    PXL_20241008_012759888.jpg
    1.4 MB
View attachment 65224 can somebody please tell me what I have in solution? This is a status chloride test That I used on a catalytic converter. Substrate chlorine leach solution!
Welcome to us.
Set things aside and study first, salts from PGM solutions are exceedingly toxic and needs proper protective gear and good lab hygiene to do.
And even then it is much better to smelt them than leach them.

Anyway, your pictures and description do not provide enough information to let us help you.

Here are some links that you need to study:
We ask our new members to do 3 things.
1. Read C.M. Hokes book on refining jewelers scrap, it gives an easy introduction to the most important chemistry regarding refining.
It is free here on the forum: https://goldrefiningforum.com/phpBB3/viewtopic.php?f=54&t=19798
2. Then read the safety section of the forum: https://goldrefiningforum.com/forums/safety.47/
3. And then read about "Dealing with waste" in the forum: https://goldrefiningforum.com/threads/dealing-with-waste.10539/

Suggested reading:
https://goldrefiningforum.com/forums/the-library.101/
https://goldrefiningforum.com/threads/when-in-doubt-cement-it-out.30236/
https://goldrefiningforum.com/threa...le-read-this-before-you-post-about-ore.33333/