1.I had about 70 Processors around 370 grams after removing the copper heat pipes
2.Since i did not know the problems with having too much nitric acid in the solution around 600 ml of AR 3:1 rookie method
3.I used Urea for denoxing which was also poor choice i would have used sulfamic acid since i did not know the problems at the time .
4.I used 2 beakers one with 200 ml of the solution and one with 400 ml of the solution since i knew something can go wrong
5. After it stopped dissolving urea which was also probably too much according to what i think after adding SMB brown yellowish gas releases and the solution turns dark for few seconds then starts turning green And a lot of foaming .
6.Now from what i have gathered i maybe accidentally made dangerous substance because solution is light
Green and has thick foam at the bottom of the solution
7. Now after knowing what i have done i am kind of afraid how do i treat it off i have kept it at a well ventilated seprate room .
Is there anything i can do safely treat it off
8. Is white residue at bottom is the potentially dangerous part can i filter the rest of the solution to another flask and deal with that later after i know exactly what i am doing
Kindly Guide me to deal with it safely
Thank you
Apologies
2.Since i did not know the problems with having too much nitric acid in the solution around 600 ml of AR 3:1 rookie method
3.I used Urea for denoxing which was also poor choice i would have used sulfamic acid since i did not know the problems at the time .
4.I used 2 beakers one with 200 ml of the solution and one with 400 ml of the solution since i knew something can go wrong
5. After it stopped dissolving urea which was also probably too much according to what i think after adding SMB brown yellowish gas releases and the solution turns dark for few seconds then starts turning green And a lot of foaming .
6.Now from what i have gathered i maybe accidentally made dangerous substance because solution is light

7. Now after knowing what i have done i am kind of afraid how do i treat it off i have kept it at a well ventilated seprate room .
Is there anything i can do safely treat it off
8. Is white residue at bottom is the potentially dangerous part can i filter the rest of the solution to another flask and deal with that later after i know exactly what i am doing