I have quartz stone and I'm sure it contains gold but I'm unaware of the percentages of the minerals in it. I crushed the stone to small granules. I cleaned the crushed resultant using nitric acid with heating then I executed another cleaning process using normal tab water. Then again I cleaned the mixture with sulfuric acid then washed the mixture with water.
Finally after all this cleaning process, i prepared my aqua regia solution using the percentage of 1 nitric acid to 3 HCL in a glass container and then added my mixture of crushed granules to the glass container of aqua regia solution and then I heated the solution just before the solution boils, let the solution cool down a bit then heat again.
After the dissolving process, i filtered my mixture to remove the impurities and have a clean aqua regia.
Then I neutralized the nitric acid in the aqua regia using urea with heat.
My issue is that when I neutralize, the solution takes up so much urea until the reaction stops.
Then I try to precipitate using SMB but there is no gold precipitation and the color of the solution dims.
Then when i leave the solution and check it after a day, the solution's color sometimes lightens up a little bit.
Can you please advise us on what we could be doing wrong in any of the steps above?
Finally after all this cleaning process, i prepared my aqua regia solution using the percentage of 1 nitric acid to 3 HCL in a glass container and then added my mixture of crushed granules to the glass container of aqua regia solution and then I heated the solution just before the solution boils, let the solution cool down a bit then heat again.
After the dissolving process, i filtered my mixture to remove the impurities and have a clean aqua regia.
Then I neutralized the nitric acid in the aqua regia using urea with heat.
My issue is that when I neutralize, the solution takes up so much urea until the reaction stops.
Then I try to precipitate using SMB but there is no gold precipitation and the color of the solution dims.
Then when i leave the solution and check it after a day, the solution's color sometimes lightens up a little bit.
Can you please advise us on what we could be doing wrong in any of the steps above?