I have some material that I need help with im willing to send a piece of it if you are willing to refining it I want to know how much gold is in it.want more info contact me please help.
As Eaglekeeper says, images and a roughly position might work to draw interest.I have some material that I need help with im willing to send a piece of it if you are willing to refining it I want to know how much gold is in it.want more info contact me please help.
If you inform the forum of the nearest city and take a few pictures of the item.It's from a x-ray tube housing.i work in a recycle center so it's not brass or bronze
It's from a x-ray tube housing.i work in a recycle center so it's not brass or bronze
I work in a recycle center so it's not brass or bronze
Okay, on the XRF.No on the XRF and negative no smoke at all
What did the stannous test say before adding smb?It did this when I added the smb is it normal?
The composition of your material may have Molybdenum, Cadmium, Lead, Tungsten an some other material as well...information taken from google when i wrote "Xray tube housing"It did this when I added the smb is it normal?