PRECIOUS METALS Well-known member Joined Feb 28, 2007 Messages 116 Location HOLLYWOOD,CA Mar 16, 2007 #1 sold out
lazersteve Well-known member Joined Feb 27, 2007 Messages 7,334 Location Florida Mar 16, 2007 #2 I PM'd you.
Noxx Well-known member Joined Feb 24, 2007 Messages 3,365 Location Quebec, Canada Mar 16, 2007 #3 I did too !
PRECIOUS METALS Well-known member Joined Feb 28, 2007 Messages 116 Location HOLLYWOOD,CA Mar 25, 2007 #4 i got lots of 10 lbs for 250.00 plus 20 dollers shipping
A Anonymous Guest Jul 15, 2007 #5 Doe anyone know an approximate yeild on 10lbs of these pins? Please advise. Regards, Rick
lazersteve Well-known member Joined Feb 27, 2007 Messages 7,334 Location Florida Jul 15, 2007 #6 Rick, You can expect these pins to yield between 0.75 g and 1.25 g per pound with 1.0 g being the average. I managed to get my hands on 11# of them, so I'll get to posting some yields for them one of these days. Steve
Rick, You can expect these pins to yield between 0.75 g and 1.25 g per pound with 1.0 g being the average. I managed to get my hands on 11# of them, so I'll get to posting some yields for them one of these days. Steve
PRECIOUS METALS Well-known member Joined Feb 28, 2007 Messages 116 Location HOLLYWOOD,CA Jul 16, 2007 #7 i still got 10 pounds left