creth
Member
Does anyone have a guessimate of the amount of gold, and silver in 1 pound of CPU's. I was thinking between 1/4 - 1/2 oz of both, but haven't done any refining to learn yet. thanks for any info you have.
Creth
Creth
leavemealone said:Hey barren,can you convert this for me please?I formatted 2 weeks ago and lost excel.If not can you(or someone else) open it and paste it please(or email it to me)?I want to compare notes.
Thanks guys,
Johnny
What am I looking at here frank?How about some Pentium Pro's.
Thanks jim,I am trying that now......nice to see you.It's been a while.Johnny,
You can just download open office.That's what I use.
Jim
leavemealone said:What am I looking at here frank?How about some Pentium Pro's.
Thanks jim,I am trying that now......nice to see you.It's been a while.Johnny,
You can just download open office.That's what I use.
Jim
Johnny
Sweet,you should have around 22-23 grams there.That is 50 Pentium Pro CPU's