Topher_osAUrus said:I dont pay alot for them at all.
The plating is "thicker" but it still doesn't hold its foil shape if processed in nitric. Another downside, is since HGE is usually 18k or 24k its rubbed off the exterior much easier (the ones I see always have wear spots down to bare metal)
So they are a sulfuric cell or cyanide candidate.
I usually pay 5 or 10 bucks a pound for HGE stuff.
Have yet to get an "exact" yield on them, because I just run them in my sulfuric cell with all my other plated and costume stuff.
I too would like to know if I am paying too much.