lioser,
Welcome to the Gold Refining Forum! We are glad to have you here. This forum contains some of the most experienced and knowledgeable members when it comes to refining precious metals from various forms of stock. This is a self help forum. What that means is there is a bit of self education required before the seasoned members here are more interested in helping you with questions and guidance. Below is a checklist that should be completed for your safety, the safety of those around you and property.
1. I would recommend you stop everything you are doing and read Refining Precious Metal Wastes by C.M. Hoke. Below is a link to a thread, here in our forum, where you can download a free copy.
http://www.scribd.com/doc/2815953/Refining-Precious-Metal-Wastes-C-M-Hoke
Reference the post by one of our most knowledgeable members, "jimdoc"
jimdoc
Active Member
Posts: 3524
Joined: March 12th, 2007, 9:42 pm
Location: Philadelphia
2. You should perform the acquaintance experiments Ms. Hoke instructs, to better familiarize yourself with the different type of reactions different metals have with different acids and temperatures. However, before performing any exercise, review the MSDS Sheet for each acid in the exercise.
3. I would learn what the scientific names are for different acids. For instance, you should learn that Hydrogen Peroxide is also known as H2O2. Also learn the chemical symbols for different elements like Platinum, which is also known as Pt.
Once all of the above have been completed, you should then thoroughly go through the Welcome Tutorial thread located at the link below AND read through all the sections of the forum, in its entirety:
http://goldrefiningforum.com/phpBB3/viewtopic.php?p=6873#6873
Our seasoned members here will know if you have done your homework and if you know the material from Hoke's book, Refining Precious Metals Wastes. Their willingness to help you greatly depends on their belief that you have successfully completed all of the above.
We are glad to have you!