Andyhaynes
Member
- Joined
- Feb 20, 2018
- Messages
- 9
I am a newb for sure. I added too much nitric acid to the aqua Regia. Everything went into solution. It created a very dark liquid. I added a little sulfuric acid to try to get the silver and lead out and filtered it out. I added more fingers until I saw some of the gold leaf floating. I assumed I had added enough material in solution. I then filtered out the remaining materials. And added SMB and left it for several days. The liquid is green and what I think is silver chloride crystals on the bottom. I checked the solution before adding smb with stanous chloride and it showed gold. After smb I’m not getting any sign. Can anyone help?
Thanks
Andy