Yes, I have read that they use high alkaline solutions to dissolve quarts, and it can also apparently dissolve some of the tin oxides.Why do you want to boil it in Potassium Carbonate?
Do you hope to dissolve the Tin?
If this were the case, it would make separating the gold from the final heavy sands a pretty easy task.