I have this stone and I crushed it and made a powder out of it, I used aqua regia to it and waited for 1 day, after that I filtered the solution and followed some steps of youtubers to get rid of the nitric oxide and other excess nitric ions on it and I boiled the solution that i filtered and added some urea to it while boiling after that the solution turned black and I worried that it fails so I added a bit of diluted smb to it and small amount of distilled water I boiled it for awhile and I got this please help me if this is correct. I don't have stannous chloride to check whether there's a gold in it but it now there's small brown sands that precipitated at the bottom. As you can see from the photo, it doesn't clung just a sand pls help.
 

Attachments

  • 307264735_397547515897226_6624533661537494027_n.jpg
    307264735_397547515897226_6624533661537494027_n.jpg
    82.4 KB
  • 298015441_1145042169434195_8252583092821909532_n.jpg
    298015441_1145042169434195_8252583092821909532_n.jpg
    83.8 KB

Latest posts

Back
Top