Wilton David
Member
Hello everyone, greetings from Ecuador, my English is not good and I use a translator to learn more about this forum, my question is how can I make my silver cleaner? I have around 800 grams and I mixed it with nitric acid which has a blue color and my question is what can I do to make it come out better quality, thank you very much for your comments.
The method I use is to add salt (sodium chloride), stir well with a wooden tube and wait for it to settle, pour out the acid and I am left with a white material that is like cheese, then I add floor shavings that replace the steel or aluminum nails and I proceed to dry and melt in fire, but I would like to improve the quality of my silver, thank you for your time.
The method I use is to add salt (sodium chloride), stir well with a wooden tube and wait for it to settle, pour out the acid and I am left with a white material that is like cheese, then I add floor shavings that replace the steel or aluminum nails and I proceed to dry and melt in fire, but I would like to improve the quality of my silver, thank you for your time.