Impurities of NaOCN and K4Fe(CN)6 in sodium cyanide.

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

Stowmaster

Well-known member
Joined
Dec 10, 2011
Messages
48
Please tell me, whether you can use for gold cyanide leaching mixture containing NaCN+KCN and impurities NaOCN+KOCN (max 25%) and K4Fe(CN)6 (max 10%)? Can these impurities to spoil the process?
 
They sure can spoil the process--you'd be well-served not to have the iron in there (which makes it harder to recover).


L
 

Latest posts

Back
Top