I have been busy on other projects, but am circling back to some 18k that I need to inquart first. My question stems from my necessity to refine the inquarted Au with poorman's AR. I understand that inquarting using 92.5% silver (sterling) may be a better way to proceed.
Then when I use the Poorman's AR to refine the 6k I expect to encounter silver chloride. This will be difficult to filter or decant out. Any advice?
From previous refines I have been reserving the silver chloride until I have enough to use the NaOH and Karo method, but this is uncharted territory for me. Any suggestions would be appreciated.
Thanks
I have been busy on other projects, but am circling back to some 18k that I need to inquart first. My question stems from my necessity to refine the inquarted Au with poorman's AR. I understand that inquarting using 92.5% silver (sterling) may be a better way to proceed.
Then when I use the Poorman's AR to refine the 6k I expect to encounter silver chloride. This will be difficult to filter or decant out. Any advice?
From previous refines I have been reserving the silver chloride until I have enough to use the NaOH and Karo method, but this is uncharted territory for me. Any suggestions would be appreciated.