I had always heard that inquarting with copper could be done so I tried it and it worked beautifully.
I'd have to say that it cleaned the gold up better than inquarting with silver.
But, since I refine silver also, I'll stick with using silver.
For the benefit of those who might not have access to silver, here's the video: