I've been a gold miner for over thirty years. I recently found what I believe is a pgm nickel ore I need an assayer that can handle all phms and gold. I'll post a couple of pics. I also gave it the h202 3% test. Which it passed with fizzing . A positive sign for platinum
 

Attachments

  • IMG_20240612_102801427.jpg
    IMG_20240612_102801427.jpg
    679.2 KB · Views: 0
  • IMG_20240612_102642559.jpg
    IMG_20240612_102642559.jpg
    675.8 KB · Views: 0
I've been a gold miner for over thirty years. I recently found what I believe is a pgm nickel ore I need an assayer that can handle all phms and gold. I'll post a couple of pics. I also gave it the h202 3% test. Which it passed with fizzing . A positive sign for platinum
Welcome to us.
Read this first:
https://goldrefiningforum.com/threa...s-before-you-post-about-ore.32137/post-341903

Next, Hydrogen Peroxide is
unstable and there are very many substances that will make it fizz.
So that is not a good testing method.
 