Hi Everyone,
I have this nugget of PM, I got it checked by a local platinum dealer and they gave me an XRF report(attached) that indicates I have 71% Ir and 8% Rh. I am in Ontario, Canada. Does anyone know how do I go about selling this ?
 

Attachments

  • IMG_8092.jpg
    IMG_8092.jpg
    2.8 MB · Views: 133
  • IMG_8091.jpg
    IMG_8091.jpg
    2.9 MB · Views: 133
  • IMG_8069.jpg
    IMG_8069.jpg
    2.5 MB · Views: 133
Where does it come from? Size? Weight?

Iridium that has been identified by xrf is usually arsenic.
See https://goldrefiningforum.com/phpBB3/viewtopic.php?f=51&t=28009&sid=64da41653eb29a8786cf9a86d2788da0

Göran
 
Origin is Spark Plugs, weight is around an oz(35.7g), size is around 1" in dia. What would you suggest instead of XRF ?
 