spaceships said:Sounds like the OP doesn't even know the product he has Kevin let alone processes, so is mentioning cyanide appropriate at this point?
Hey guys,i am a part time scraper and i dont refine,i just scrap parts and sell them to local buyer like motherbords,rams etc...now i have a car trunk of old computer cables with this pins and im interseted to pull them out insted off selling them with cables.Is it worth it?kurtak said:spaceships said:Sounds like the OP doesn't even know the product he has Kevin let alone processes, so is mentioning cyanide appropriate at this point?
And he has been a member since Oct. 8 - 2013 :?:
Kurt
Tnx Henrik great link, i have 33kg already striped connectors from cable and they are only old ones like on the photo.Its a eazy job pull them out.The new ones that are only thin caped i dont pull out and sell them as they are.canedane said:There are gold in all the pins, the old are full plated ,the newer generation is only plated in the tip.
Do not waist your time to collect the pins, they are low grade, i will guess there is from 0,2 to 0,5 g gold in one kilo of this pins.
In the long winter nights here i cut the ends of the cable,then i have copper wires readdy for sale and the connector ends can be sold to scrap compagnyes.
Here is a link to a German scrap dealer.http://badenschrott.de/e-schrott-ankaufspreise/ they pay 1.6 euro for a kilo.
Henrik
PERO said:Tnx Henrik great link, i have 33kg already striped connectors from cable and they are only old ones like on the photo.Its a eazy job pull them out.The new ones that are only thin caped i dont pull out and sell them as they are.canedane said:There are gold in all the pins, the old are full plated ,the newer generation is only plated in the tip.
Do not waist your time to collect the pins, they are low grade, i will guess there is from 0,2 to 0,5 g gold in one kilo of this pins.
In the long winter nights here i cut the ends of the cable,then i have copper wires readdy for sale and the connector ends can be sold to scrap compagnyes.
Here is a link to a German scrap dealer.http://badenschrott.de/e-schrott-ankaufspreise/ they pay 1.6 euro for a kilo.
Henrik
So even old ones are not bother to pull out?
Tnx again Henrik for link and u maybe know buyer like this closer to Austrija?Im from Slovenia and looking to min distance to sell scrap when i open my scrap company next month.
chears
silversaddle1 said:While not an expert on plating, I thought pins were plated with nickel before gold. If that's true then any part of the pin that is not gold plated would be silver. Seems brass would be a poor choice for this type of connection without some type of plating on it.
Enter your email address to join: