Friends, first, I added ammonia solution to the AR , it turned red, then I added HCL, the solution turned yellow, and white recipted settled under it.
 

Attachments

  • IMG_20241127_140143.jpg
    IMG_20241127_140143.jpg
    2.8 MB
Friends, first, I added ammonia solution to the AR , it turned red, then I added HCL, the solution turned yellow, and white recipted settled under it.
Two things.
Get some gloves on your hand
And as Anachrenism asked.
What was your plan about adding Ammonia to the AR solution?
What was in the AR solution in the first place?

As I can see, the main thing that happens is the release of massive amounts of Ammonia gas.
Next you push the pH of the AR up so unknown Hydroxides form.
If that was the plan, you have succeeded.

Seriously, what about forming a plan and ask if that plan makes sense?
 
Friends, first, I added ammonia solution to the AR , it turned red, then I added HCL, the solution turned yellow, and white recipted settled under it.
I know I am quite sarcastic now.
But I'm out of tools on how to get through to you.
Do you have any ideas on what works to get your attention?
 