Hi, i am new on the forum, but i did a little research before i posted and didn't find a post about the pins on the motherboard that have pins on wich the jumper is put, they are long and square after removal.
And also the conectors on the motherboard in wich the cd rom and floppy etc fit in are the same after removal, i would like to know a aproximate yeld per kilo or lb, Thank's alot. :D
 
Use the "Search" to find what you are looking for. There are several posts about them on here. They are gold plated but the yield would depend on the thickness of the plating which can be very thin. It will take several ounces of them to amount to very much gold. Many of the jumpers also contain gold plating on the inside.
Claude
 