Hello everyone!
I just began processing pin (very small amount to give my plan a go)
Equipment (safety is accounted for)
1. Hotplate
2. Sodium nirate
3. 32% HCL
4. Distilled water
5. Stannous test
my plan was to just use poor mans aqua regia to dissolve twice however maybe i should have given a HCL bath first to remove more base metals. I wanted to stop because there were a few unknowns.
steps i did:
1.Mix of 125 ml hcl 32%
2. 28 g NaNO3
3. 100 ml H20
4. Add my pins
5. After my reaction stopped i ended up with gold floating on top and some gold on pins.
6. Did a stannous test and no gold in solution.
Questions:
1.should I do another poorman aqua regia run after decanting and filtering?
2. What is the white powder at the bottom?
3. My stannous chloride is light blue - it cannot be palladium or silver can it?
I just began processing pin (very small amount to give my plan a go)
Equipment (safety is accounted for)
1. Hotplate
2. Sodium nirate
3. 32% HCL
4. Distilled water
5. Stannous test
my plan was to just use poor mans aqua regia to dissolve twice however maybe i should have given a HCL bath first to remove more base metals. I wanted to stop because there were a few unknowns.
steps i did:
1.Mix of 125 ml hcl 32%
2. 28 g NaNO3
3. 100 ml H20
4. Add my pins
5. After my reaction stopped i ended up with gold floating on top and some gold on pins.
6. Did a stannous test and no gold in solution.
Questions:
1.should I do another poorman aqua regia run after decanting and filtering?
2. What is the white powder at the bottom?