This is what I found today. Haven’t tried it yet trying to find correct solution for Nitric acid and Poor Mans AR
Have Gallon of mureactic acid and Hi-Yield Ammonia calcium nitrate in pellet form fertilizer.
 

Attachments

  • 8F2CB233-13DC-4ABF-B140-510ADBFDDFE2.png
    8F2CB233-13DC-4ABF-B140-510ADBFDDFE2.png
    353.5 KB
  • 0C43B927-1A5F-4326-9246-1EC2451473AA.png
    0C43B927-1A5F-4326-9246-1EC2451473AA.png
    364.6 KB
This is what I found today. Haven’t tried it yet trying to find correct solution for Nitric acid and Poor Mans AR
Have Gallon of mureactic acid and Hi-Yield Ammonia calcium nitrate in pellet form fertilizer.
For poormans AR there is no problem.
With poormans Nitric it will create gypsum.
It is important to know the difference between the two.
One is just HCl and Nitrate the other is Sulfuric and Nitrate.
 
Hello again as I was earlier in my post I had a couple buckets that sat over winter. Two days ago I mixed Mureactic acid and just let it sit. This is what was at bottom of the bucket. Any help would be appreciated as to what to do with this.

Thanks Brad
 

Attachments

  • 855C369B-3064-45F1-BF5A-6E97EF8755F6.jpeg
    855C369B-3064-45F1-BF5A-6E97EF8755F6.jpeg
    211.7 KB
  • 39629471-CAE8-4727-AB02-DC960223DDCA.jpeg
    39629471-CAE8-4727-AB02-DC960223DDCA.jpeg
    206.1 KB
Most likely Copper (i) Chloride aka Cuprous Chloride, a salt of copper. It forms when copper is dissolved in HCl with insufficient oxygen to form Copper (ii) Chloride aka Cupric Chloride. It is toxic so don't throw it in the trash or down the drain.
 