Lead wheel weights have been outlawed in most States and Provinces, Zinc is being used as one alternative. The tires shops near my home have been giving me their discarded weights by the bucket full over the past two years.
I decided to melt them into ingots this afternoon when I discovered about half were zinc, thought I would pass it on for those of you using zing in your refining process.
I decided to melt them into ingots this afternoon when I discovered about half were zinc, thought I would pass it on for those of you using zing in your refining process.