I have been throwing my cards (video, network, modem etc) and memory in a box once I have removed the fingers. My question is what is the best thing to do with these cards once I am done with them. Is there any place that buys them for the remainder of the values I did not get? The wife wants them out of the garage. Thanks you.
 
My buyer buys them, he may downgrade them to $1 per pound from $1.70 per pound if the fingers are cut off. But that is better than trashing them.The memory with fingers off he pays around $3 per pound. Jim
 
Gold Trail said:
Jim doc, ever try dealing with ARM in philly?
No I haven't. I have had a guy from Jersey contact me, but never
got any pricing info from him. Things have been very slow, and the stuff I have been getting is too nice to scrap. I would rather see old beat up stuff that I wouldn't think twice about scrapping. But lately I have been getting nice P4 machines. I deal with this guy;
http://thriftybits.com/
Jim
 