Hi Kurt.....
Now when you find boards like these - that is when you find boards that are AMAZING supper high grade & a jackpot you get once in awhile

Kurt

1699563055485.png


I have several items like yours in this picture . How did you process them ? Sulphuric Stripping Cell?
 
Hi. They are not pcb's - they are large copper blocks (hard to see it from the picture). I understand how to process the pcb's in AP. Thank you.
 

Attachments

  • IMG_0903.JPG
    IMG_0903.JPG
    884 KB
Last edited:
Hi. They are not pcb's - they are large copper blocks (hard to see it from the picture). I understand how to process the pcb's in AP. Thank you.
The all metal ones can be done in a Sulfuric cell.
The PCB's in AP, Nitric or even Cyanide if you can access it and follow protocols strictly.
 