Hello ,
People who understand the process are designing and building packaged turnkey units
and charging a lot of money for them. I built a blast furnace for under $800 in Hong Kong and could have easily
it for $2700.00 or more. It accomadated #30 Morgan clay graphite crucibles that could pour 1000 ounces Ag.
At Wesgo Metals in Belmont we used to use CoorsTec Evaporation dishes on gas fired hotplates inside
of custom built fume hoods connected to a $1,000,000.00 acid gas scrubing system. We also had
double jacketed glass lined Phaudler reactors connected to the scrubber.
I have been looking around a while and find this gold refining machinery very appealing and
I I know that the procedures, (not the machinery) could easily be reproduced at a fraction
of the cost simply starting with the items below.
You can set up your own turnkey refinery
PPE, Personel protective equipment
Security
Vault
Benches
A Fume Hood
Acid Gas Scrubber
Stirrer Hot Plates
Wash Bottles 250 - 500 ml
Deionized Water Filtration System
Heavy Duty Pyrex Beakers
30 Gallon PPL Cooling and Precipitation Tanks
Filter Funnel CoorsTec
Filter Adapers
Filtrate Flasks Just a simple 5 or 6 gallon glass water bottle can be used with a funnel adaptor
Bulk Chemicals
Electric Kiln or Big torch, Blast Furnace or Induction Furnace
Crucible and Tongs
Iron Molds
Shot Tank
Number and Letter Stamps
Easy
I am working on a gold and silver refining blog and constantly updating it.
Visit Gold and Silver Refining Supplies Blog...
for more info: http://GoldandSilverRefinerySupplies.Blogspot.Com
Thanks
Steve Looser
ΩPhoenix Consulting
©2012 All rights reserved
People who understand the process are designing and building packaged turnkey units
and charging a lot of money for them. I built a blast furnace for under $800 in Hong Kong and could have easily
it for $2700.00 or more. It accomadated #30 Morgan clay graphite crucibles that could pour 1000 ounces Ag.
At Wesgo Metals in Belmont we used to use CoorsTec Evaporation dishes on gas fired hotplates inside
of custom built fume hoods connected to a $1,000,000.00 acid gas scrubing system. We also had
double jacketed glass lined Phaudler reactors connected to the scrubber.
I have been looking around a while and find this gold refining machinery very appealing and
I I know that the procedures, (not the machinery) could easily be reproduced at a fraction
of the cost simply starting with the items below.
You can set up your own turnkey refinery
PPE, Personel protective equipment
Security
Vault
Benches
A Fume Hood
Acid Gas Scrubber
Stirrer Hot Plates
Wash Bottles 250 - 500 ml
Deionized Water Filtration System
Heavy Duty Pyrex Beakers
30 Gallon PPL Cooling and Precipitation Tanks
Filter Funnel CoorsTec
Filter Adapers
Filtrate Flasks Just a simple 5 or 6 gallon glass water bottle can be used with a funnel adaptor
Bulk Chemicals
Electric Kiln or Big torch, Blast Furnace or Induction Furnace
Crucible and Tongs
Iron Molds
Shot Tank
Number and Letter Stamps
Easy
I am working on a gold and silver refining blog and constantly updating it.
Visit Gold and Silver Refining Supplies Blog...
for more info: http://GoldandSilverRefinerySupplies.Blogspot.Com
Thanks
Steve Looser
ΩPhoenix Consulting
©2012 All rights reserved