hi every one, it is just an effort to move on. i am a small scale home refiner from 2 years, but nit very old on this forum. i am looking forward from small to mid refininer, i am always intrested in making own things. so i am going to start to show what i want to do and what i will do to make a medium setup for ewaste processing.
so from start,
scrap to be recycle!
1 motherboards( non chinese, old stuff)
2 rams( all types)
3 old HDR boards,
4 processers( non ceramic)
5 mobile boards( old)
Mathod of saperation
manual depopulation with hammer chisel
saperation
ics(all types)+ mlccs+ processors
so first step is to make a pyroliser. from many ideas imon forum i decided to use this design
need comments on this so design should be change or upgrade for more effeciency as many master minds hidden on forum
so from start,
scrap to be recycle!
1 motherboards( non chinese, old stuff)
2 rams( all types)
3 old HDR boards,
4 processers( non ceramic)
5 mobile boards( old)
Mathod of saperation
manual depopulation with hammer chisel
saperation
ics(all types)+ mlccs+ processors
so first step is to make a pyroliser. from many ideas imon forum i decided to use this design
need comments on this so design should be change or upgrade for more effeciency as many master minds hidden on forum