Please tell me what you think. I thought it was a broken sandstone slab. But to my surprise it was heavy and broken on one side revealing metallic patterning incased in copper maybe.
Hard to say without further information.Please tell me what you think. I thought it was a broken sandstone slab. But to my surprise it was heavy and broken on one side revealing metallic patterning incased in copper maybe.
Hmm I see you have posted this in the Rogues Gallery.Please tell me what you think. I thought it was a broken sandstone slab. But to my surprise it was heavy and broken on one side revealing metallic patterning incased in copper maybe.
Welcome to usStrongly suggest slag from furnace.
Rob.
Looks more like a piece of Lead/Zinc replacement ore in limestone. Is it magnetic? If so, it could be Magnetite. Another way to test is for a Whitmenstat pattern. I doubt it is a meteorite by its shape, but who knows, until you have it authenticated, which you will not get at this forum.Please tell me what you think. I thought it was a broken sandstone slab. But to my surprise it was heavy and broken on one side revealing metallic patterning incased in copper maybe.
Enter your email address to join: