- Joined
- Aug 12, 2021
- Messages
- 1,261
Does anybody know of a company that sells either slides with accurate size graduations, or the scope with a built in graduation, to measure the size of a tiny prill? For those that don't know, Gold has a characteristic that makes it almost perfectly round, when reduced in a cupel. For super tiny beads, which would normally require a super accurate scale (= expensive). A cheaper solution can be to use either the above, or a micrometer. Thanks in advance.