0,24 gramm
silver-palladium alloy 80/20.
The middle contact (normally open) is just a solid piece.
everything is silvered on top.
The thickness of the silver plating is visible after the burner.
people knew how to do 50 years ago.
:)
 

Attachments

  • IMG_20241120_192507914_MP.jpg
    IMG_20241120_192507914_MP.jpg
    1.1 MB
  • IMG_20241120_192455408_MP.jpg
    IMG_20241120_192455408_MP.jpg
    1.3 MB
  • IMG_20241120_193442661_MP.jpg
    IMG_20241120_193442661_MP.jpg
    201.3 KB
  • IMG_20241120_193455981_MP.jpg
    IMG_20241120_193455981_MP.jpg
    1.3 MB
  • IMG_20241120_193754639_MP.jpg
    IMG_20241120_193754639_MP.jpg
    167.3 KB
  • IMG_20241120_193650618_MP.jpg
    IMG_20241120_193650618_MP.jpg
    148.9 KB
  • IMG_20241120_193803295_MP.jpg
    IMG_20241120_193803295_MP.jpg
    167.1 KB
  • IMG_20241120_194131082_MP.jpg
    IMG_20241120_194131082_MP.jpg
    4.1 MB
Whenever I see a component which is the "wrong" color, I dig a little deeper. Microrelays, for example, are a pain to scrap, but when I do, it seemed like all the orange ones had gold plated silver alloy. And it's neat to have a soft fluffy ball of copper wire from the coil!
 
Those may be "signal" relays, which jogged my memory, I have 2000+ of these and arthritis in both my thumbs.
Gold-clad silver says the datasheet.
 

Attachments

  • Panasonic Aromat lr26550 TN2E-4.5V b.png
    Panasonic Aromat lr26550 TN2E-4.5V b.png
    21.1 KB
  • IMG_20240801_170506a.jpg
    IMG_20240801_170506a.jpg
    447.5 KB
  • IMG_20240801_170035.jpg
    IMG_20240801_170035.jpg
    703.8 KB
  • IMG_20240801_170005.jpg
    IMG_20240801_170005.jpg
    699.9 KB
  • IMG_20240801_165704.jpg
    IMG_20240801_165704.jpg
    594.9 KB
  • Panasonic Aromat lr26550 TN2E-4.5V .png
    Panasonic Aromat lr26550 TN2E-4.5V .png
    160 KB
Back
Top