W wokaway Member Joined Aug 8, 2014 Messages 6 Feb 10, 2015 #1 Hi all, Are these these blocks in the centre of the cpu mlcc's? And will they contain palladium? Thanks Alastair Attachments image.jpg 41.8 KB
Hi all, Are these these blocks in the centre of the cpu mlcc's? And will they contain palladium? Thanks Alastair
FrugalRefiner Administrator Staff member Administrator Supporting Member Moderator Joined Jan 14, 2012 Messages 6,726 Location Ohio, USA Feb 10, 2015 #2 wokaway said: Are these these blocks in the centre of the cpu mlcc's? Click to expand... Yes. And will they contain palladium? Click to expand... Maybe. Welcome to the forum. Not all MLCCs contain silver and/or palladium. Dave
wokaway said: Are these these blocks in the centre of the cpu mlcc's? Click to expand... Yes. And will they contain palladium? Click to expand... Maybe. Welcome to the forum. Not all MLCCs contain silver and/or palladium. Dave