Hello everybody!
My name is Arturs, i am 30 year old, from Latvia - tiny country in East Europe, Baltics, have background in entrepreneurship.
some time ago i got obsessed with the idea of e-waste recycling (i think from some youtube videos), so i started collecting old PC and other e-scrap, somewhat recently i found this forum and started studying, got hokes book also
Thanks to this forum and all you guys posting i made my first button few days ago (1.919 grams), got it XRF`d at the local university, it tested at 95% Au, so i guess i am still in the recovery realm for now still not so bad for working in the middle of field, with few mason jars, without any previous expirience.
it was pretty challenging and i am quite proud of myself, i am yet not convinced that there is real possibility for a succesfull bussines to be made there for me, though, but still for now I would wery much like to be a part of this great forum
Thanks again for this amazing place, could not have done it without you guys, thank all of you!
P.s. i hope it is not against rules to post a picture of my buttons:
My name is Arturs, i am 30 year old, from Latvia - tiny country in East Europe, Baltics, have background in entrepreneurship.
some time ago i got obsessed with the idea of e-waste recycling (i think from some youtube videos), so i started collecting old PC and other e-scrap, somewhat recently i found this forum and started studying, got hokes book also
Thanks to this forum and all you guys posting i made my first button few days ago (1.919 grams), got it XRF`d at the local university, it tested at 95% Au, so i guess i am still in the recovery realm for now still not so bad for working in the middle of field, with few mason jars, without any previous expirience.
it was pretty challenging and i am quite proud of myself, i am yet not convinced that there is real possibility for a succesfull bussines to be made there for me, though, but still for now I would wery much like to be a part of this great forum
Thanks again for this amazing place, could not have done it without you guys, thank all of you!
P.s. i hope it is not against rules to post a picture of my buttons: