I would like to thank you all and this great forum. These are my humble buttons refined only by inquartation.

I hope to refine using AR in the near future.
 

Attachments

  • IMG_20170627_111528.jpg
    IMG_20170627_111528.jpg
    460.1 KB · Views: 372
  • IMG_20170702_174901.jpg
    IMG_20170702_174901.jpg
    311.6 KB · Views: 372
  • IMG_20170808_205442.jpg
    IMG_20170808_205442.jpg
    1.5 MB · Views: 372
  • IMG_20170808_205600.jpg
    IMG_20170808_205600.jpg
    1.2 MB · Views: 372
  • IMG_20170906_160439.jpg
    IMG_20170906_160439.jpg
    1.7 MB · Views: 372
That first button in particular is a great example of just how pure the gold can be from inquartation and nitric leaching.

You should wear gloves when refining to avoid those stains on your hands.

Dave
 
Nice button. However, it does look like it wasn't fully melted on the bottom. Almost look like powder on your palm. Are those stains? If so, you should be wearing gloves messing with acids. Looks like Nitric stains.

scrapparts
 
Thanks guys!

That first button in particular is a great example of just how pure the gold can be from inquartation and nitric leaching.

You should wear gloves when refining to avoid those stains on your hands.

Dave

Nice button. However, it does look like it wasn't fully melted on the bottom. Almost look like powder on your palm. Are those stains? If so, you should be wearing gloves messing with acids. Looks like Nitric stains.

scrapparts


-- Yes Dave, once in a while I get high purity buttons just by nitric. Maybe it depends upon the contaminants because these gold I get here is of different ore types.

-- scrapparts those buttons are fully melted. Those are stains from silver nitrate.

--I am using gloves while refining but I always manage to get stains upon fixing the containers.

cheers!
 
by autumnwillow » October 13th, 2017, 7:49 am

Sell them to me! =D

I would love to sell them to you sir autumn but I have a tight situation with my capital right now. For this, I have to refine and sell here immediately for the money to be used again for buying.

But eventually I will have a transaction with you again soon sir autumn,.that's for sure.

By the way how is everything there?


by anachronism » October 6th, 2017, 2:26 pm

Nothing humble at all about those buttons Sir. Great job.

You guys here make my buttons humble sir anachronism :D
 
Everything is good. I have a friend who lives in your area whom I can entrust a transaction with. He usually comes over to my place every 2 weeks or so. That way, you'll have a faster turn around. Let me know if you are interested.
 