HAY GUY'S THIS IS MY VERY FIRST BUTTON OOOO YEA !!!! LOL

I can't get the pic to post so im going to email it to steve so my be he can for me sorry!!
I got yep yep!!!

lazersteve said:
Here it is Chris, Good Work!! Tell us more about it!

here a link
 
Congrats. It sure looks a lot better than my 1st one. I used no flux.

It came from 30 fiber CPU's in AR.

Laugh if Ya want!
 

Attachments

  • Funky Nugget.jpg
    Funky Nugget.jpg
    55.8 KB · Views: 672
It came from cpu fingers, pins, and crushed scraps from computer parts. I processed it using AR. I have a little more from when I did my test batch. It is not much, it was all fingers.

About 5lb or so, I think could be more.
 